ECS Transactions, The Electrochemical Society, Vol. 16, No. 49 ( 2009-08-29), p. 469-477
Abstract:
The current efficiency for NF3 formation was investigated using Boron-Doped Diamond (BDD) anode in NH4F·nHF melts. It depended on both the current density and the NH4F-concentration. The best current efficiency was obtained at 40 mA/cm2 and the NH4F-concentration of 33.3 mol% (the NH4F·2HF melt), and its value was 72.4%.