    In:  International Polymer Processing Vol. 17, No. 4 ( 2002-12-01), p. 333-338
    In: International Polymer Processing, Walter de Gruyter GmbH, Vol. 17, No. 4 ( 2002-12-01), p. 333-338
    Kurzfassung: In this study, various effects on the properties of the material, such as free-radical (FR) processes, oxygen induction time (OIT), melting temperature and melting heat are examined during several stages of the polyethylene (PE) pipe extrusion process. The spectra in the Electron Spin Resonance (ESR) are researched between 77–293 K and in a wide range of magnetic fields. At 77 K a triplet signal in ESR is observed. The parameters of the signal are ΔH m1 ≅ 1:4 – 1:6 mT; ΔH m2 ≅ 1 – 1:2 mT; ΔH m3 ≅ 0:6 – 0:8 mT and g 1 ≅ 2:020; g 2 ≅ 2:011; g 3 ≅ 1:99 and Hyper Fine Structure constant ΔH 12 ≅ 2:1 mT; ΔH 23 ≅ 5:3 mT. As the temperature increase from 77 K up to 293 K, the signal for g 4 ≅ 2:02 (ΔH m 4 ≅ 0:7 – 0:8 mT) appears and intensity of signals increase. It is also thought that the triplet observed at 77 K belongs to macroradicals of alkyl (–CH 2 –CH–CH 2 ), alyl(~CH 2 C HCH = CHCH 2 ~), carboanions and the acyl (H C O) radicals of the fourth signal. At room temperature, all the FR's transform into peroxide radicals. The total concentration of the FR's is minimum at 463 K and increases at the outlet of the extruder and the pipe sample. It is observed that the OIT (Oxygen Induction Time) values decrease as one approaches the outlet of the extruder (from 20–30 to 10–15 minutes), while they increase for the processes of 433 K to 463 K. This event proves that the peroxide radicals form as one passes to room temperature. These results support those of the effects of the extrusion stage on the dynamic-mechanical characteristics [2]. Finally, FR's appear as a result of the breaking of the C-C bonds in the main polymer chains starting from the first step in the extrusion process (433 K) and in the later stages, due to the oxygen in the polymer structure, oxidation processes take place.
    Materialart: Online-Ressource
    ISSN: 2195-8602 , 0930-777X
    Sprache: Englisch
    Verlag: Walter de Gruyter GmbH
    Publikationsdatum: 2002
    Bibliothek Standort Signatur Band/Heft/Jahr Verfügbarkeit
    BibTip Andere fanden auch interessant ...
Schließen ⊗
Diese Webseite nutzt Cookies und das Analyse-Tool Matomo. Weitere Informationen finden Sie auf den KOBV Seiten zum Datenschutz