Abstract:
The anodic aluminum oxide (AAO) films were prepared by anodization method from the 15 vol. % sulphuric acid solution, and prepared AAO films were heat-treated in the ranges of 25~1000°C. AAO films were characterized by EDAX, SEM and XRD techniques, respectively. The crystal phases of prepared AAO film is amorphous. The apertures of AAO film are in 25~30 nm. AAO films are amorphous when heat treatment temperatures of AAO films are below 800 °C. After the AAO film being heat-treated in the ranges of 850°C~900 °C, the heat-treated AAO film are γ-Al 2 O 3 film. When the AAO film is heat-treated at 950 °C, the part of γ-Al 2 O 3 change into α-Al 2 O 3 , and the heat-treated AAO film are mixed film of γ-Al 2 O 3 and α-Al 2 O 3 . After the AAO film being heat-treated at 1000 °C, the heat-treated AAO film is α-Al 2 O 3 film.
Type of Medium:
Online Resource
ISSN:
1662-7482
DOI:
10.4028/www.scientific.net/AMM.577
DOI:
10.4028/www.scientific.net/AMM.577.11
Language:
Unknown
Publisher:
Trans Tech Publications, Ltd.
Publication Date:
2014
detail.hit.zdb_id:
2251882-4