In:
Advanced Materials Research, Trans Tech Publications, Ltd., Vol. 833 ( 2013-11), p. 295-300
Abstract:
The glass powder as a binder phase in the silver paste mainly plays the role of binding. The composition, content and particle size of the glass powder have significant effects on the properties of the silver paste. In this paper, the effects of the sintering temperature, holding time, glass powder content and glass powder size on the adhesion and square resistance of the silver film were studied. The research results showed that when the glass powder content was 6%(in mass) of the total silver paste, the sintering temperature was 680°C, the holding time was 7 minutes and the glass powder size was 2.47μm, the silver paste can get good properties. The adhesion strength and square resistance of the silver film were respectively 2.5 N/mm 2 and 14 mΩ /.
Type of Medium:
Online Resource
ISSN:
1662-8985
DOI:
10.4028/www.scientific.net/AMR.833
DOI:
10.4028/www.scientific.net/AMR.833.295
Language:
Unknown
Publisher:
Trans Tech Publications, Ltd.
Publication Date:
2013
detail.hit.zdb_id:
2265002-7