Materials Science Forum, Trans Tech Publications, Ltd., Vol. 852 ( 2016-4), p. 811-815
Abstract:
Si/C composite was prepared using different procedures and different C sources in this work. According to the electrochemical performances, it was found that the discharge capacity for Si/C composite (SC1) by the electrostatic spinning procedure using polyvinylpyrrolidone as the C source was 2200mAh/g. In contrast, the cell with the pure Si particle exhibited an initial discharge capacity of only 13mAh/g. Moreover, after 30 cycles, SC1 sample had the higher capacities and the better capacity retention performances than other samples because of its lower charge transfer resistance. The inclusion of carbon not only worked as a stable electric conductive pathway but also buffer the volume expansion of the silicon during the process of charging and discharging.
Type of Medium:
Online Resource
ISSN:
1662-9752
DOI:
10.4028/www.scientific.net/MSF.852
DOI:
10.4028/www.scientific.net/MSF.852.811
Language:
Unknown
Publisher:
Trans Tech Publications, Ltd.
Publication Date:
2016
detail.hit.zdb_id:
2047372-2